PARFIX 3203 is a medium viscosity combined with fast cure speed, and excellent thermal resistant cyanoacrylate adhesive. It is modified cyanoacrylate adhesive with improved resistance to heat, humidity or damp environments. It is specifically formulated to bond various Rubbers, Metals and Plastics for use in challenging environments. Applications: - Ideal for bonding Rubbers, Metals and Plastics.
- Excellent hot strength and heat aging capabilities at temperatures up to 120°C for periods in excess of 3000 hours.
- Ideal for Speaker Assemblies, Automotive Components, Electrical Equipment, Oil Filters and Disk Drives.
Information provided by Parson Adhesives, Inc. |