MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bostik EzPoxy™ Epoxy Mortar & Grout
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: Bostik® EzPoxy™ 100% Solids Epoxy Mortar & Grout is installations. Typical applications include commercial and residential kitchens, lobbies, bathrooms, fast food restaurants, breweries, dairies, wineries, factories, shopping malls, meat processors, and distilleries. Meets ANSI A118.3.

Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.00 %
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 5000 psi
Shear Strength 1000 psi
@Time 605000 sec
Ceramic Mosaic, Bond
 1000 psi
@Time 605000 sec
Quarry Tile, Bond
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 - 24.0 hour
Pot Life 45.0 min
Shelf Life 12.0 Month
 
Descriptive Properties
Installation Temperature50-90°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bostik QuartzLock2™ RapidCure™ Urethane Grout
Bostik NeverSeal™ Grout
Concrete, Lightweight
Bostik Dimension® RapidCure™ Grout
Bostik 425 Acrylic Latex

PBOSTK008 / 191544

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.