MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Coating P. Materials EB-92AS TPU for Film and Sheet
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: CPMC produces and specializes on TPU materials for film and sheet use, which is widely processing in common use and increase working efficiency. TPU apply to film and sheet with good characteristics including as below,+ Process easily+ Endurance at low temperature and maturing)

Product Description: Water vapor permeability type, excellent water resistance, nice touch, good physical properties and elasticity. Good fluidity, well controlled viscosity, good workability etc.

Application To End-Use Products: Shoe products, clothes, medical supplies, industrial goods and baby products

Information provided by Coating P. Materials Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 88 - 92ASTM D2240
Tensile Strength 330 kg(f)/cm²ASTM D412
Elongation, Ultimate 600 %ASTM D412
100% Modulus 90.0 kg(f)/cm²ASTM D412
300% Modulus 150 kg(f)/cm²ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTCOAT029 / 293973

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.