MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Petropol Nypol® A3 G10 NTLA010 NR452 Nylon 66, 10% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Polyamide 6.6 natural reinforced with 10% of fiberglass, good set of thermal and mechanical properties. Ideal for injection molding.

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ASTM D792
Water Absorption 2.22 %2.22 %Humidity Absorption; ASTM D570
 7.1 %7.1 %ASTM D570
Maximum Moisture Content 0.200.20
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inASTM D955
Deformation 1.1 %
@Pressure 27.6 MPa,
Temperature 50.0 °C
1.1 %
@Pressure 4000 psi,
Temperature 122 °F
ASTM D621
Ash 8.0 - 12 %8.0 - 12 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 118 MPa17100 psiASTM D638
Tensile Strength 120 MPa17400 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
 3.2 %3.2 %Strain at Break; ASTM D638
Tensile Modulus 5.50 GPa798 ksiASTM D638
Flexural Strength 190 MPa27600 psiASTM D790
Flexural Modulus 5.30 GPa769 ksiASTM D790
Shear Strength 75.0 MPa10900 psiASTM D732
Izod Impact, Notched 0.480 J/cm0.899 ft-lb/inASTM D256
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
ASTM D256
 4.50 kJ/m²
@Temperature 23.0 °C
2.14 ft-lb/in²
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched (ISO)  35.0 kJ/m²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
ASTM D256
 40.0 kJ/m²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ASTM D256
Charpy Impact Unnotched  3.00 J/cm²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
ASTM D256
 3.20 J/cm²
@Temperature 23.0 °C
15.2 ft-lb/in²
@Temperature 73.4 °F
ASTM D256
Charpy Impact, Notched  0.400 J/cm²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
ASTM D256
 0.450 J/cm²
@Temperature 23.0 °C
2.14 ft-lb/in²
@Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 250 - 265 °C482 - 509 °FASTM D2217
Deflection Temperature at 1.8 MPa (264 psi) 230 °C446 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 - 280 °C500 - 536 °FMolding
Mold Temperature 65.0 - 120 °C149 - 248 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL108 / 313016

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.