Notes: Elexar® EL-1934G is a high performance UL V-0 flame retardant thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Elexar EL-1934G is a high hardness, high density, high flow grade that is UV stabilized and RoHS compliant. This UL listed grade is easily colorable and is suitable for both molding and extrusion. Features: Chemical Resistant; Filled; Flame Retardant; Good Adhesion: Good Colorability; Good Flexibility; Good Moldability; Good Processability; Good Toughness; High Density; High Specific Gravity; Low Flow; Medium Hardness; Sunlight Resistant (720 hours); UV Resistant; Weather Resistant Uses: Cable Jacketing; Electrical/Electronic Applications; Industrial Applications; Insulation; Wire & Cable Applications; Wire Jacketing Form: Pellets Processing Method: Extrusion; Injection Molding Information Provided by Teknor Apex |