MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
PolyMirae Adstif HA686J Thermoforming, EBM Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: Adstif HA686J is New Generation Thermoforming Grade for SPPF made by Basell“new process and additive formulation technology". So, this product shows higher stiffness, impact strength, HDT, and better clarity than General Homo T/F grade. In addition, because Adstif HA686J is Homo PP, this product has better stretchability than General Homo T/F grade [So, suitable for SPPF(Solid Phase Pressure Forming) T/F application]. Adstif HA686J resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact.

Product Features: Very good stiffness/Good top load strength/Good clarity/Good processability and stretchability /Low odor and taste transfer/ Hot fillable/ microwavable for reheating of foods

Typical Applications: Drinking cups/ Yogurt cups/ Noodle cups/ Margarine tubs/ Dairy cups/ Various trays for food/ EBM bottle/etc

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASMT D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108ASTM D785
Tensile Strength, Yield 370 kg(f)/cm²ASTM D638
Elongation at Yield 10 %ASTM D638
Flexural Modulus 17800 kg(f)/cm²ASTM D790
Izod Impact, Notched 4.80 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 125 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accucomp Polypropylene HPO306L Homopolymer
PolyMirae Adstif HA748L Injection Molding Grade Polypropylene
PolyMirae Adstif EA640G High stiffness sheet Polypropylene Copolymer
Polykemi AB SCANFILL FOIL ABYX52C1 PP/PE, Thermoforming Grade
Pinnacle Polymers 1402 C Clarified Polypropylene Homopolymer Thermoforming Grade

PMIRAF35 / 183256

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.