A high-purity version of 3M™ Novec™ 7200, 3M™ Novec™ 7200DL is tightly-controlled for ions, metals and non-volatile residue. It is used when an application calls for high-purity materials, or a higher boiling point is desirable Feature and Benefits: - Non-flammable
- Non-conductive
- Compatible with plastics
- Low toxicity
- Low Global Warming Potential (GWP)
- Zero ozone depletion potential
- VOC-exempt solvent (US EPA)
- Low surface tension penetrates tight spaces for improved cleaning
- High purity for sensitive applications
Information provided by 3M |