MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) AvaSpire® AV-651 GF50 Polyaryletherketone (PAEK), 50% glass fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Glass Fiber Filled

Material Notes: AvaSpire® AV-651 GF50 is a 50% chopped glass fiber-reinforced polyaryletherketone (PAEK) resin. It has been specifically formulated to provide exceptionally high strength and stiffness at elevated temperatures along with very strong chemical resistance to a broad range of harsh chemical environments encountered across a wide variety of industries and engineering applications. Typical potential applications for AV-651 GF50 include orthopedic and dental instruments, under-the-hood automotive parts, and parts in the chemical and oil and gas industries. This grade is easily injection moldable into precision molded parts.

Typical property data provided are based on a limited production history.

- Beige: AvaSpire® AV-651 GF50 BG 20
- Black: AvaSpire® AV-651 GF50 BK 95

Applications: Aircraft Applications; Automotive Applications; Connectors; Dental Applications; Electrical/Electronic Applications; Hospital Goods; Industrial Applications; Medical Devices; Medical/Healthcare Applications; Seals; Surgical Instruments

Features: Autoclave Sterilizable; Biocompatible; Chemical Resistant; E-beam Sterilizable; Ethylene Oxide Sterilizable; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; Good Sterilizability; Heat Sterilizable; High Heat Resistance; High Stiffness; High Strength; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam Sterilizable

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.73 g/ccASTM D792
Water Absorption 0.10 %
@Time 86400 sec
ASTM D570
Viscosity 630 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
Melt; ASTM D3835
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 400 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 199 MPa5.0 mm/min; ASTM D638
Elongation at Break 2.1 %5.0 mm/min; ASTM D638
Tensile Modulus 17900 MPa5.0 mm/min; ASTM D638
Flexural Strength 297 MPaASTM D790
Flexural Modulus 16500 MPaASTM D790
Izod Impact, Notched 110 J/mASTM D256
Izod Impact, Unnotched 960 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 340 °CPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 287 °C
@Thickness 3.20 mm
Annealed; ASTM D648
Glass Transition Temp, Tg 158 °CDSC
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 365 °C
Middle Barrel Temperature 371 °C
Front Barrel Temperature 377 °C
Nozzle Temperature 382 °C
Melt Temperature 366 - 388 °CInjection
Mold Temperature 160 - 190 °C
Drying Temperature 149 °C
@Time 14400 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBeige; Black
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion
Screw Compression Ratio2.0:1.0 to 3.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4153 / 279953

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.