Design/Construction: Side 1: Uncured Silicone Rubber Substrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone Rubber Side 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass cloth This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications. Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation. |