MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Sarlink® TPV 24587 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink 24587 is a high performance thermoplastic vulcanizate used in automotive and consumer/industrial applications. This product is a high hardness, low density, lubricated grade exhibiting excellent tear strength. This grade suitable for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Filled; Good Moldability; Good Processability; Good Tear Strength; High Hardness; Light Stabilized; Low Density; Low Flow; Low Specific Gravity; Lubricated

Uses: Expansion Joint; Gaskets; Grommets; Plugs; Shock Absorbing Pads; Tubing; Weatherstripping

Agency Ratings: UL 94

RoHS Compliance: RoHS Compliant

UL File Number: QMFZ2.E54709

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ISO 1183
Viscosity 264 cP
@Shear Rate 206 1/s,
Temperature 200 °C
264 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Apparent; ASTM D3835
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  86
@Time 15.0 sec
86
@Time 0.00417 hour
Injection Molded; ISO 868
 87
@Time 5.00 sec
87
@Time 0.00139 hour
Injection Molded; ISO 868
 90
@Time 1.00 sec
90
@Time 0.000278 hour
Injection Molded; ISO 868
 86.1
@Treatment Temp. 110 °C,
Time 15.0 sec
86.1
@Treatment Temp. 230 °F,
Time 0.00417 hour
Injection Molded, Change in Air, 1008; ISO 888
 86.1
@Treatment Temp. 125 °C,
Time 15.0 sec
86.1
@Treatment Temp. 257 °F,
Time 0.00417 hour
Injection Molded, Change in Air, 168; ISO 888
 87.2
@Treatment Temp. 110 °C,
Time 5.00 sec
87.2
@Treatment Temp. 230 °F,
Time 0.00139 hour
Injection Molded, Change in Air, 1008; ISO 888
 87.2
@Treatment Temp. 125 °C,
Time 5.00 sec
87.2
@Treatment Temp. 257 °F,
Time 0.00139 hour
Injection Molded, Change in Air, 168; ISO 888
 90.5
@Treatment Temp. 110 °C,
Time 1.00 sec
90.5
@Treatment Temp. 230 °F,
Time 0.000278 hour
Injection Molded, Change in Air, 1008; ISO 888
 90.5
@Treatment Temp. 125 °C,
Time 1.00 sec
90.5
@Treatment Temp. 257 °F,
Time 0.000278 hour
Injection Molded, Change in Air, 168; ISO 888
Tensile Strength at Break 9.17 MPa1330 psiAcross Flow, Type 1, 20 in/min; ISO 37
 12.1 MPa1750 psiFlow, Type 1, 20 in/min; ISO 37
 9.10 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
1320 psi
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Type 1, Change in Air; ISO 188
 9.27 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
1340 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Type 1, Change in Air; ISO 188
 11.8 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
1710 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Flow, Type 1, Change in Air; ISO 188
 13.2 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
1910 psi
@Treatment Temp. 257 °F,
Time 168 hour
Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain  5.77 MPa
@Strain 100 %
837 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 8.41 MPa
@Strain 100 %
1220 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 6.46 MPa
@Strain 100 %,
Treatment Temp. 110 °C
937 psi
@Strain 100 %,
Treatment Temp. 230 °F
Across Flow, Type 1, Change in Air in 1008 hr; ISO 188
 6.52 MPa
@Strain 100 %,
Treatment Temp. 125 °C
946 psi
@Strain 100 %,
Treatment Temp. 257 °F
Across Flow, Type 1, Change in Air in 168 hr; ISO 188
 10.0 MPa
@Strain 100 %,
Treatment Temp. 110 °C
1450 psi
@Strain 100 %,
Treatment Temp. 230 °F
Flow, Type 1, Change in Air in 1008 hr; ISO 188
 11.2 MPa
@Strain 100 %,
Treatment Temp. 125 °C
1620 psi
@Strain 100 %,
Treatment Temp. 257 °F
Flow, Type 1, Change in Air in 168 hr; ISO 188
Elongation at Break 440 %440 %Flow, Type 1, 20 in/min; ISO 37
 470 %470 %Across Flow, Type 1, 20 in/min; ISO 37
 299 %
@Treatment Temp. 125 °C,
Time 605000 sec
299 %
@Treatment Temp. 257 °F,
Time 168 hour
Flow, Type 1, Change in Air; ISO 188
 352 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
352 %
@Treatment Temp. 230 °F,
Time 1008 hour
Flow, Type 1, Change in Air; ISO 188
 385 %
@Treatment Temp. 125 °C,
Time 605000 sec
385 %
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Type 1, Change in Air; ISO 188
 425 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
425 %
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Type 1, Change in Air; ISO 188
Tear Strength 45.6 kN/m260 pliMethod Ba, Angle (Unnicked), Flow, 20 in/min; ISO 34-1
 73.6 kN/m420 pliMethod Ba, Angle (Unnicked), Across Flow, 20 in/min; ISO 34-1
Compression Set  32 %
@Temperature 22.8 °C,
Time 79200 sec
32 %
@Temperature 73.0 °F,
Time 22.0 hour
Type A; ISO 815
 49 %
@Temperature 70.0 °C,
Time 79200 sec
49 %
@Temperature 158 °F,
Time 22.0 hour
Type A; ISO 815
 58 %
@Temperature 90.0 °C,
Time 252000 sec
58 %
@Temperature 194 °F,
Time 70.0 hour
Type A; ISO 815
 76 %
@Temperature 125 °C,
Time 252000 sec
76 %
@Temperature 257 °F,
Time 70.0 hour
Type A; ISO 815
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 50.0 °C122 °FUL 746
UL RTI, Mechanical with Impact 50.0 °C122 °FUL 746
UL RTI, Mechanical without Impact 50.0 °C122 °FUL 746
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
All Colors
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 230 °C374 - 446 °FInjection, Melt
Rear Barrel Temperature 173 - 213 °C344 - 416 °FInjection
Middle Barrel Temperature 179 - 219 °C354 - 426 °FInjection
Front Barrel Temperature 184 - 224 °C364 - 436 °FInjection
Nozzle Temperature 190 - 230 °C374 - 446 °FInjection
Zone 1 166 - 204 °C330 - 400 °FExtrusion
Zone 2 171 - 210 °C340 - 410 °FExtrusion
Zone 3 177 - 216 °C350 - 420 °FExtrusion
Zone 4 179 - 218 °C355 - 425 °FExtrusion
Zone 5 182 - 221 °C360 - 430 °FExtrusion
Die Temperature 190 - 227 °C374 - 440 °FExtrusion
Mold Temperature 35.0 - 60.0 °C95.0 - 140 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 120 rpm50 - 120 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1194 / 237685

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.