System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LG Chemical SG175G ABS, Super Surface Gloss, High Flow
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Molded
Material Notes:
Feature: Injection Molding, Super Surface Gloss, High Flow
Application: Electric & Electronic Products
CAS No. 9003-56-9
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.04
g/cc
1.04
g/cc
ASTM D792
Maximum Moisture Content
0.010
0.010
Injection Molding
Linear Mold Shrinkage, Flow
0.0040
-
0.0070
cm/cm
@Thickness 3.20 mm
0.0040
-
0.0070
in/in
@Thickness 0.126 in
ASTM D955
Melt Flow
37
g/10 min
@Load 10.0 kg,
Temperature 220 °C
37
g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
108
108
ASTM D785
Tensile Strength, Yield
46.1
MPa
@Thickness 3.20 mm
6680
psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break
30 %
@Thickness 3.20 mm
30 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Yield
>= 5.0 %
@Thickness 3.20 mm
>= 5.0 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Yield Strength
73.5
MPa
@Thickness 3.20 mm
10700
psi
@Thickness 0.126 in
15 mm/min; ASTM D790
Flexural Modulus
2.55
GPa
@Thickness 3.20 mm
370
ksi
@Thickness 0.126 in
15 mm/min; ASTM D790
Izod Impact, Notched
2.26
J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
4.22
ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
2.35
J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
4.41
ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+16
ohm-cm
1.00e+16
ohm-cm
Dielectric Strength
28.0
kV/mm
711
kV/in
Arc Resistance
60
-
120
sec
60
-
120
sec
ASTM D495
Comparative Tracking Index
>=
600
V
>=
600
V
Solution A; IEC 60112
Hot Wire Ignition, HWI
7.0
-
15
sec
@Thickness >=1.50 mm
7.0
-
15
sec
@Thickness >=0.0591 in
15
-
30
sec
@Thickness >=3.00 mm
15
-
30
sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI
30
-
60
arcs
@Thickness 1.50 mm
30
-
60
arcs
@Thickness 0.0591 in
>=
120
arcs
@Thickness 3.00 mm
>=
120
arcs
@Thickness 0.118 in
High Voltage Arc-Tracking Rate, HVTR
10.0
-
25.4
mm/min
0.394
-
1.00
in/min
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
85.0
°C
@Thickness 6.40 mm
185
°F
@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point
92.0
°C
@Load 5.00 kg
198
°F
@Load 11.0 lb
50°C/h; ASTM D1525
UL RTI, Electrical
60.0
°C
@Thickness >=1.50 mm
140
°F
@Thickness >=0.0591 in
UL 746B
60.0
°C
@Thickness >=3.00 mm
140
°F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact
60.0
°C
@Thickness >=1.50 mm
140
°F
@Thickness >=0.0591 in
UL 746B
60.0
°C
@Thickness >=3.00 mm
140
°F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact
60.0
°C
@Thickness >=1.50 mm
140
°F
@Thickness >=0.0591 in
UL 746B
60.0
°C
@Thickness >=3.00 mm
140
°F
@Thickness >=0.118 in
Flammability, UL94
HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
HB
@Thickness >=3.00 mm
HB
@Thickness >=0.118 in
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
180
-
200
°C
356
-
392
°F
Injection Molding
Middle Barrel Temperature
190
-
210
°C
374
-
410
°F
Injection Molding
Front Barrel Temperature
200
-
220
°C
392
-
428
°F
Injection Molding
Nozzle Temperature
200
-
230
°C
392
-
446
°F
Injection Molding
Melt Temperature
210
-
240
°C
410
-
464
°F
Injection Molding
Mold Temperature
40.0
-
70.0
°C
104
-
158
°F
Injection Molding
Drying Temperature
80.0
°C
176
°F
Injection Molding
Dry Time
2.00
-
4.00
hour
2.00
-
4.00
hour
Injection Molding
Back Pressure
29.4
-
58.8
MPa
4260
-
8530
psi
Injection Molding
Screw Speed
30
-
60
rpm
30
-
60
rpm
Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
LG Chemical HG173 ABS, High Surface Gloss
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance
LG Chemical LUPOY GP1000M PC, Transparent
LG Chemical TR557 MABS, High Transparency, High Impact
PTS Trilac® ABS-HS6500 High Impact ABS Resin
PLAY024 / 148032
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.