MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Haynes Hastelloy® W alloy, gas metal arc welds, as-welded
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemical process industries.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: AWS A5.14, ASME SFA 5.11, ASME SFA 5.14, AMS 5755, AMS 5786, AMS 5787, AWS A5.11
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 9.00 g/cc0.325 lb/in³at RT
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 870 MPa126000 psi
 310 MPa
@Temperature 870 °C
45000 psi
@Temperature 1600 °F
Tensile Strength, Yield 555 MPa80500 psi
 285 MPa
@Temperature 870 °C
41300 psi
@Temperature 1600 °F
Elongation at Break 38 %38 %
 41 %
@Temperature 870 °C
41 %
@Temperature 1600 °F
Reduction of Area 32 %32 %
 42 %
@Temperature 870 °C
42 %
@Temperature 1600 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.2 µm/m-°C
@Temperature 20.0 - 600 °C
7.33 µin/in-°F
@Temperature 68.0 - 1110 °F
 13.2 µm/m-°C
@Temperature 20.0 - 500 °C
7.33 µin/in-°F
@Temperature 68.0 - 932 °F
 13.5 µm/m-°C
@Temperature 20.0 - 700 °C
7.50 µin/in-°F
@Temperature 68.0 - 1290 °F
 14.2 µm/m-°C
@Temperature 20.0 - 800 °C
7.89 µin/in-°F
@Temperature 68.0 - 1470 °F
 14.8 µm/m-°C
@Temperature 20.0 - 900 °C
8.22 µin/in-°F
@Temperature 68.0 - 1650 °F
 15.3 µm/m-°C
@Temperature 20.0 - 1000 °C
8.50 µin/in-°F
@Temperature 68.0 - 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.12 %<= 0.12 %
Chromium, Cr 5.0 %5.0 %
Cobalt, Co 2.5 %2.5 %
Iron, Fe 6.0 %6.0 %
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 24 %24 %
Nickel, Ni 63 %63 %
Silicon, Si <= 1.0 %<= 1.0 %
Vanadium, V <= 0.60 %<= 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haynes Hastelloy® C-2000® alloy, flat products
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 65% Cold Reduction
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 55% Cold Reduction
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction
Carlson C 600 Nickel-Chromium-Iron Alloy

NHAWAE / 16998

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.