MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

P & P Technology A320C UL Neoprene/EPDM
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: SAE J18 Specification: 2C2
ASTM Specification: 2C2 (1985&91). SCE42 (1967&68). RE42E1 (1978)
Flame Resistance: Pass UL94V-0, HBF, HF-1**, GM609OMB4,A FMVSS302 Pass @ 0.8mm.
IMDS Node ID: 13900758

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.0864 - 0.1056 g/cc0.0864 - 0.1056 g/cc
Water Absorption <= 0.050 %<= 0.050 %
 0.10 %0.10 %Allowed
Deformation 25 %
@Pressure 0.00345 - 0.0621 MPa
25 %
@Pressure 0.500 - 9.01 psi
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 5050
Tensile Strength >= 0.827 MPa>= 120 psi
Elongation at Break >= 150 %>= 150 %
Compression Set <= 12.5 %<= 12.5 %D3575; 0.5
 <= 25 %<= 25 %D1056; 0.5
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 110 °C230 °F
Minimum Service Temperature, Air -42.0 °C-43.6 °F
Flammability, UL94 V-0V-0
Shrinkage <= 5.0 %
@Temperature 70.0 °C,
Time 605000 sec
<= 5.0 %
@Temperature 158 °F,
Time 168 hour
Heat Ageing Lineal
 
Descriptive Properties
Fluid Immersion<250%ASTM E, Fuel B
Heat Ageing Max Change3057 days @ 70°C
Ozone Resistance Rating0'72 hrs @ 50pphm, ASTM D1171

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polykemi AB POLYfill PP EIP8020F Polypropylene/EPDM, Mineral Reinforced
Ethylene Propylene Rubber (EPM, EPDM)
Armacell Monarch® F-03091 (Black) Pure EPDM Foam
Eurofoam Porocell POR 445 CDN CR-Neoprene Foam
Garlock 244 Neoprene Rubber - Commercial Grade

PPPTEC032 / 133496

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.