MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 204 GB FR Nylon 6/6 (PA), Glass Bead - Flame Retardant - UL94 V-0
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Bead Filled

Material Notes: RTP 204 GB FR is a flame retardant, nylon 6.6 containing 25% glass beads. It is characterized by excellent moldability, warp resistance, thermal stability, and is non-corrosive.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.61 g/ccASTM D 792
Water Absorption 0.70 %
@Time 86400 sec
ASTM D 570
Additive Loading 25 %Primary Additive
Linear Mold Shrinkage 0.011 - 0.016 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D 785
Tensile Strength at Break 10000 psiASTM D 638
Elongation at Break 2.0 - 3.0 %ASTM D 638
Tensile Modulus 700 ksiASTM D 638
Flexural Strength 17000 psiASTM D 790
Flexural Modulus 700 ksiASTM D 790
Izod Impact, Notched 0.700 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 6.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmASTM D 257
Dielectric Constant 4.2
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 475 V/milShort Term; In Oil; ASTM D 149
Dissipation Factor 0.015
@Frequency 1e+6 Hz
Dry; ASTM D 150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 490 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 360 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
Oxygen Index 33 %ASTM D 2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 530 - 570 °F
Mold Temperature 150 - 225 °F
Drying Temperature 175 °F
@Time 14400 sec
Moisture Content 0.20 %
Dew Point 0.000 °F
Injection Pressure 10000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® TR 90 PAMACM12
EMS-Grivory Grilamid® TR 90 LS PAMACM12
EMS-Grivory Grilamid® LVX-50H black 9230 PA12-GF50
RTP Company RTP 200 H FR Impact-Modified Nylon 6/6 (PA), High Impact - Unreinforced - Flame Retardant - UL94 V-0
Polyram PlusTek PA340S05 Nylon 6.6 for Injection Molding, 5% Glass-beads Reinforced, Heat Stabilized

PQZWA900 / 92454

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.