MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LEXAN™ Copolymer FXE1414L Polycarbonate (PC) (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consult CIC or PM for color availability & limitation.

Features: High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.28 g/cc1.28 g/ccASTM D792
Density 1.28 g/cc0.0462 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.0700 %0.0700 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.17 %0.17 %ISO 62-1
Viscosity 10 cP
@Load 1.20 kg,
Temperature 300 °C
10 cP
@Load 2.65 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 11 g/10 min
@Load 1.20 kg,
Temperature 300 °C
11 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 47.0 MPa6820 psi50 mm/min; ISO 527
 54.0 MPa7830 psi50 mm/min; ASTM D638
Tensile Strength, Yield 52.0 MPa7540 psi50 mm/min; ASTM D638
 52.0 MPa7540 psi50 mm/min; ISO 527
Elongation at Break 75 %75 %50 mm/min; ISO 527
 84 %84 %50 mm/min; ASTM D638
Elongation at Yield 5.0 %5.0 %50 mm/min; ASTM D638
 5.0 %5.0 %50 mm/min; ISO 527
Tensile Modulus 2.00 GPa290 ksi1 mm/min; ISO 527
 2.03 GPa294 ksi50 mm/min; ASTM D638
Flexural Strength 83.0 MPa12000 psiyield, 2 mm/min; ISO 178
 86.0 MPa12500 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.05 GPa297 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.11 GPa306 ksi2 mm/min; ISO 178
Izod Impact Notched 766 J565 ft-lbASTM D256
 640 J
@Temperature -30.0 °C
472 ft-lb
@Temperature -22.0 °F
ASTM D256
Dart Drop, Total Energy 68.0 J50.2 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 70.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  67.3 µm/m-°C
@Temperature -40.0 - 40.0 °C
37.4 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 82.3 µm/m-°C
@Temperature -40.0 - 40.0 °C
45.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 118 °C244 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 121 °C
@Thickness 3.20 mm
250 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 138 °C280 °FRate B/50; ISO 306
 138 °C280 °FRate B/50; ASTM D1525
 146 °C295 °FRate B/120; ISO 306
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94 HB
@Thickness 0.400 mm
HB
@Thickness 0.0157 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 290 - 310 °C554 - 590 °F
Zone 2 280 - 305 °C536 - 581 °F
Zone 3 295 - 315 °C563 - 599 °F
Melt Temperature 295 - 315 °C563 - 599 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80276 / 288223

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.