General purpose economy grade copolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for maximum weatherability. Available in Natural and Black. Natural: Designated R190H2-N3; Black: Designated R190-H2B. Data provided by the manufacturer |
Ashley Polymers, Inc.; Polyoxymethylene (POM) |