MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Baydur® STR/C 1000 Liquid Structural RIM
Categories: Fluid

Material Notes: Characterization: Baydur STR/C-1000 is a moderate-viscosity, two-component, liquid structural RIM (reaction injection molding) system.

Properties / Applications: Baydur STR/C-1000 is moderate-viscosity, two-component, liquid structural RIM (reaction injection molding) system. Component A is a modified polymeric diphenylmethane diisocyanate (PMDI) blend,and Component B is a totally formulated polyol blend. The Baydur STR/C-1000 system is used in the production of structural composite parts with long-fiber reinforcements. The reinforcement is placed in the mold, which is closed and then injected with the reactive resin. Baydur STR composites can be ten times stiffer than Baydur structural foams and have the excellent impact properties traditionally associated with Bayer polyurethanes. As with any product, use of the Baydur STR/C-1000 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccPolyol (Component B)
 1.19 g/ccASTM D1622
 1.24 g/ccIsocyanate (Component A)
Viscosity 320 cPIsocyanate (Component A)
 700 cPPolyol (Component B)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 73.8 MPaASTM D638
Elongation at Break 14 %ASTM D638
Flexural Strength 139 MPaASTM D790
Flexural Modulus 3520 MPaASTM D790
Izod Impact, Notched 1.40 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Flash Point 143 °CPolyol (Component B)
 213 °CIsocyanate (Component A)
 
Processing PropertiesOriginal ValueComments
Mold Temperature 79.0 - 88.0 °C
Gel Time 0.600 min
 
Descriptive Properties
AppearanceClear to straw yellow liquidPolyol (Component B)
 Dark brown liquidIsocyanate (Component A)
Content27.3%NCO, Isocyanate (Component A)
Hydroxyl number[mg KOH/g], Polyol (Component B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Prism® CM-200 Polyurethane Solid RIM, MDI-based 2-Component Liquid System
Covestro Baydur® STR/C 1000 Liquid Structural RIM, 30% Glass Filled
Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System
Covestro Bayflex® WR-20 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System

PCOVEST0103 / 201886

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.