Introduction: It is a two component room temperature vulcanizing pourable fluid silicon which cures on the addition of the appropriate CATALYST AD, according to the polyaddition process. SILIMOLD AD 10 silicon rubber is characterized by its low hardness and a high tearing resistance. Thanks to these properties, it may also be utilized in the manufacture of complex moulds with many undercuts. Application: SILIMOLD AD 10 silicon rubber is especially designed for complex moulds, model prototype and mould making. Pad printing. Peculiarities: Addition cure; Easy pour able; High tear strength; Extreme mould release/mould life Note 1: Tests have been carried out under these conditions: Temperature: +20°C; After: 24 ore; R.H.: 60%; Catalysis: 100:10 Information provided by Poolkemie |