System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Lubrizol Pearlbond™ 5717 NT2 Thermoplastic Polyurethane
Categories:
Polymer
;
Thermoplastic
;
Polyurethane, TP
Material Notes:
Type: Pearlbond™ 5717 NT2 is a Polyester-Type Thermoplastic Polyurethane (TPU).
Description: Hot Melt Adhesive with a low melting range.
Uses: Extrusion, powder coating.
Information provided by The 159 Corporation
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.19
g/cc
ASTM D-792
Maximum Moisture Content
0.020
Melt Flow
10
-
20
g/10 min
@Load 2.16 kg,
Temperature 160 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Hardness, Shore A
70
ASTM D-2240
Tensile Strength at Break
10.0
psi
ASTM D-412
Elongation at Break
750 %
ASTM D-412
50% Modulus
2.00
MPa
@Strain 50 %
ASTM D-412)
100% Modulus
2.50
MPa
@Strain 100 %
ASTM D-412)
300% Modulus
4.00
MPa
@Strain 300 %
ASTM D-412)
Tear Strength
30.0
kN/m
Nicked; ISO 34-1B
Thermal Properties
Original Value
Comments
Melting Point
80.0
°C
MQSA 70A
Processing Properties
Original Value
Comments
Drying Temperature
40.0
-
50.0
°C
@Time 10800 - 21600 sec
Dew Point
-40.0
°C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PLUBR5041 / 238911
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.