MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Solbrol® LB 6 Preservative
Categories: Other Engineering Material

Material Notes: Solbrol® LB 6 is a liquid blend of Dehydro Acetic Acid, Sorbic Acid and Benzoic Acid in Phenoxyethanol, that offers synergistic broad-spectrum antimicrobial protection

Application:

  • Skin care products like face creams, body lotions and others
  • Surfactant based formulations like shower gels
  • Recommend dosage: 0.2% to 1.0%
  • Recommended pH-levels below 6.5
  • Solubility in water approx. 1%, mild heating to 40 °C might be necessary

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearancePale yellow liquid, slightly viscous
Color<100Hazen
Content3.75-4.25%Sorbic acid
 5.75-6.25%Benzoic acid
 8.75-9.25%Dehydroacetic acid
 80.25-81.75%Phenoxyethanol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8166 / 208559

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.