The FG/SF series is a material solution for automotive interior applications with special surface appearance and quality requirements. It is characterized by its easy processability. The compounds are available in black. Processing Method: Injection Molding Color / RAL DESIGN: Typical applications: - Automotive Interior
- Car mats
- Function and design elements
- Soft touch for grips, switches and mats
- Soft touch surface (thumb wheels, push buttons, switches)
- Grip applications
- Bumpers
- Over molded housing
Material advantages:- Adhesion to PP
- Low density
- Abrasion resistance
- Optimized flow properties
- Non-sticky surface
- Colorable
- Controlled level of emission and odor, suitable for automotive interior
- Soft touch surface
Information provided by Kraiburg TPE |