MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sichuan Sunshine Plastics FR3090 TPV, Low smoke halogen-free fire-class
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Advantages: In wide temperature range, TPV has excellent compression and compression stress relaxation, excellent anti-aging properties and good chemical resistance, short extrusion time, light weight, and has the characteristics of 100% renewable. Products can be translucent, the color of material qualities, easy to dye and so on.

Information provided by SICHUAN SUNSHINE PLASTICS CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccGB/T1033.1-2008
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90GB/T531.1-2008
Tensile Strength 6.40 MPaGB/T528-2009
Elongation at Break 380 %GB/T528-2009
Tear Strength 58.0 kN/mGB/529-2008
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -60.0 °CGB/T1682-1994
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSICHSP012 / 314407

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.