Product Description: A soft, colorable thermoplastic vulcanizate, TPV (EPDM/PP) in the thermoplastic elastomer family offers good physical properties and chemical resistance. The Bondable to: PP, EVA, PE Availability: Africa & Middle East; Asia Pacific; Europe; North America Features: Bondability; Chemical Resistant; Ozone Resistant; Soft RoHS Compliance: RoHS Compliant Appearance: Natural Color Forms: Pellets Processing Method: Injection Molding; ExtrusionInformation provided by Elastron |