MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Trelleborg Emerson & Cuming Eccobond® D 778 One-Component Fast Cure Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Emerson & Cuming D 778 Eccobond® One-Component Fast Cure Epoxy Adhesive
High strength, semi-flexible, thixotropic, fast heat curing, epoxy structural adhesive. Good peel strength (20 pli). Recommended for reinforcing riveted or weld bonded metal panels for cabinets, buses, trailers or other sheet metal structures. Cure Type: Heat Bonding Type: Epoxy

The Eccobond® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 19.3 MPa2800 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 160 °C
0.167 hour
@Temperature 320 °F
 20.0 min
@Temperature 120 °C
0.333 hour
@Temperature 248 °F
 45.0 min
@Temperature 100 °C
0.750 hour
@Temperature 212 °F
 
Descriptive Properties
ColorYellow
ViscosityThixotropic Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEMERS72 / 35764

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.