MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

VICTREX CT™ 100 GRA Cryogenic Grade Polyetheretherketone
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, FDA food contact compliant, color natural

Typical Application Areas: Applications at very low temperatures. Wear and erosion resistant and chemically resistant to aggressive environments .

Information Provided by Victrex.

Vendors: With over 30 years of focus, experience and security of supply Victrex Polymer Solutions is the world’s leading manufacturer of high performance Polyaryletherketones (PAEK) including versatile VICTREX™ PEEK. We work with our customers and end users to deliver technology driven solutions to meet the challenges and opportunities they face and help them to achieve new levels of cost savings, quality and performance. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Drake extrudes shapes and machines and injection molds parts in Torlon® PAI, PEEK, PAEK, Ryton PPS and Ultem PEI. It also machines Vespel® PI. Innovations include cryogenic CryoDyn® CT-200 shapes as a PCTFE alternative; efficient Seamless Tube® and the largest extruded rod diameters to >254mm and plate thicknesses to > 100mm. Certified to ISO 9001:2015 and AS9100D. Visit www.DrakePlastics.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Viscosity 550000 cP
@Temperature 400 °C
550000 cP
@Temperature 752 °F
Melt; ISO 11443
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/in375°C nozzle, 180°C tool; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/in375°C nozzle, 180°C tool; ISO 294-4
Spiral Flow  19.0 cm
@Thickness 1.00 mm
7.48 in
@Thickness 0.0394 in
Mold Temp: 180°C, Melt Temp: 395°C; Victrex
 63.0 cm
@Thickness 3.00 mm
24.8 in
@Thickness 0.118 in
Mold Temp: 180°C, Melt Temp: 395°C; Victrex
 70.0 cm
@Thickness 3.00 mm
27.6 in
@Thickness 0.118 in
Mold Temp: 180°C, Melt Temp: 415°C; Victrex
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8484ISO 868
Tensile Strength at Break 200 MPa
@Temperature -196 °C
29000 psi
@Temperature -321 °F
ISO 527
Tensile Strength, Yield 95.0 MPa13800 psiISO 527
Elongation at Break  8.0 %
@Temperature -196 °C
8.0 %
@Temperature -321 °F
ISO 527
 70 %
@Temperature 23.0 °C
70 %
@Temperature 73.4 °F
ISO 527
Flexural Strength  150 MPa
@Temperature 23.0 °C
21800 psi
@Temperature 73.4 °F
ISO 178
 435 MPa
@Temperature -196 °C
63100 psi
@Temperature -321 °F
ISO 178
Flexural Modulus  3.50 GPa
@Temperature 23.0 °C
508 ksi
@Temperature 73.4 °F
ISO 178
 5.40 GPa
@Temperature -196 °C
783 ksi
@Temperature -321 °F
ISO 178
Compressive Strength  120 MPa
@Temperature 23.0 °C
17400 psi
@Temperature 73.4 °F
ISO 604
 305 MPa
@Temperature -196 °C
44200 psi
@Temperature -321 °F
ISO 604
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  42.0 µm/m-°C
@Temperature -165 °C
23.3 µin/in-°F
@Temperature -265 °F
DIN 51909
 45.0 µm/m-°C
@Temperature <=143 °C
25.0 µin/in-°F
@Temperature <=289 °F
ISO 11357-3
CTE, linear, Transverse to Flow  65.0 µm/m-°C
@Temperature <=143 °C
36.1 µin/in-°F
@Temperature <=289 °F
ISO 11357-3
 160 µm/m-°C
@Temperature >=143 °C
88.9 µin/in-°F
@Temperature >=289 °F
ISO 11357-3
Specific Heat Capacity 2.20 J/g-°C0.526 BTU/lb-°FDSC
Thermal Conductivity  0.150 W/m-K
@Temperature -165 °C
1.04 BTU-in/hr-ft²-°F
@Temperature -265 °F
Average
 0.320 W/m-K
@Temperature 23.0 °C
2.22 BTU-in/hr-ft²-°F
@Temperature 73.4 °F
Along flow; ISO 22007-4
Melting Point 343 °C649 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 163 °C325 °F(HT G22); ISO 75-f
Glass Transition Temp, Tg 143 °C289 °FOnset; ISO 11357
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 100 °C<= 212 °FHopper Temperature
Rear Barrel Temperature 375 °C707 °F
Middle Barrel Temperature 380 - 385 °C716 - 725 °F
Front Barrel Temperature 390 °C734 °F
Nozzle Temperature 395 °C743 °F
Mold Temperature 170 - 200 °C338 - 392 °F
Dry Time 3.00 - 5.00 hour
@Temperature 120 - 150 °C
3.00 - 5.00 hour
@Temperature 248 - 302 °F
Moisture Content <= 0.020 %<= 0.020 %
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ColorNatural
Gate> 1mm or 0.5 x part thickness
RunnerDie/nozzle > 3mm, manifold > 3.5mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVICTB870 / 301123

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.