Properties and applications: ACEMATT TS 100/20 is an untreated thermal silica characterized by very high matting efficiency combined with high transparency. Thanks to the unique properties, ACEMATT TS 100/20 is particularly suitable for coating systems that are difficult to matt. Special application areas include: water-based coatings, waterborne UV coatings, clear coatings, coatings for leather and films, as well as all types of top coats. Coating formulations containing ACEMATT TS 100/20 show outstanding resistance against household chemicals. The particle size distribution in ACEMATT TS 100/20 is slightly broader than in ACEMATT TS 100. ACEMATT TS 100/20 improves flow behavior and increases storage stability in powder coatings.Information provided by Evonik |