MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Samyang TRIREX® 3022IR PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Product Description: TRIREX is the registered trademark of polycarbonate resin manufactured by Samyang Corporation. TRIREX polycarbonate resins offer superior mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electronic, appliance, automotive and optical industries. TRIREX 3022IR is a polycarbonate resin grade which has high low temperature impact strength in combination with superior mechanical and physical property.
Characteristics: Superior low temperature impact resistance; Good flow-ability; Workable under a wide range of temperatures (-100-135°C); High electrical performance; Good dimensional stability; Low moisture absorbency; Good weather resistance
Applications: TRIREX 3022IR resin grade is used for electric and electronic applications, food contact materials and etc.; Medium viscosity. Transparent colors only.

Availability: Asia Pacific; Europe; North America

Features: Food Contact Acceptable; Good Dimensional Stability; Good Electrical Properties; Good Flow; Good Weather Resistance; Low Moisture Absorption; Low Temperature Impact Resistance; Medium Viscosity

Uses: Appliance Components; Automotive Applications; Electrical/Electronic Applications; Non-specific Food Applications; Optical Applications

Automotive Specifications: CHRYSLER MS-DB-145 Type A CPN4536 Color: 100% Color Match

Appearance: Clear/Transparent

Form: Pellets

Processing Method: Injection Molding

Information provided by Samyang Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption <= 0.15 %
@Time 86400 sec
<= 0.15 %
@Time 24.0 hour
ASTM D570
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.00 mm
0.0050 - 0.0070 in/in
@Thickness 0.118 in
ASTM D955
Melt Flow 14 g/10 min
@Load 1.20 kg,
Temperature 300 °C
14 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 68.9 MPa10000 psiASTM D638
Elongation at Break 130 %130 %ASTM D638
Flexural Yield Strength 93.1 MPa13500 psiASTM D790
Flexural Modulus 2.25 GPa326 ksiASTM D790
Izod Impact, Notched 9.08 J/cm
@Thickness 3.17 mm
17.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+16 ohm-cm4.00e+16 ohm-cmASTM D257
Dielectric Strength 29.9 kV/mm760 kV/inASTM D149
Arc Resistance >= 120 sec>= 120 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.4 - 70.2 µm/m-°C28.0 - 39.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 134 °C273 °FUnannealed; ASTM D648
Flammability, UL94 V-2
@Thickness 1.52 mm
V-2
@Thickness 0.0600 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 245 - 270 °C473 - 518 °F
Middle Barrel Temperature 260 - 285 °C500 - 545 °F
Front Barrel Temperature 275 - 300 °C527 - 572 °F
Nozzle Temperature 275 - 310 °C527 - 590 °F
Melt Temperature 275 - 310 °C527 - 590 °F
Mold Temperature 65.0 - 105 °C149 - 221 °F
Drying Temperature 120 °C248 °F
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hour
Back Pressure 0.250 - 0.703 MPa36.3 - 102 psi
Vent Depth 0.00201 - 0.00787 cm0.000790 - 0.00310 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSAMY11428 / 312121

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.