MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Armco 20-45-5 Iron-Nickel Alloy
Categories: Metal; Superalloy; Iron Base

Material Notes: Heat exchanger and condenser tubing, stress corrosion resistant

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Rupture Strength 5800 psi
@Temperature 816 °C,
Time 3.60e+6 sec
 8800 psi
@Temperature 816 °C,
Time 360000 sec
 11000 psi
@Temperature 732 °C,
Time 3.60e+6 sec
 16000 psi
@Temperature 732 °C,
Time 360000 sec
 23000 psi
@Temperature 649 °C,
Time 3.60e+6 sec
 32000 psi
@Temperature 649 °C,
Time 360000 sec
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.050 %
Chromium, Cr 20 %
Iron, Fe 30.37 %Balance
Manganese, Mn 4.0 %
Nickel, Ni 45 %
Niobium, Nb (Columbium, Cb) 0.15 %
Silicon, Si 0.40 %
Vanadium, V 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iron, Fe
AISI 1005 Steel
AISI 4340 Steel, normalized, 25 mm round
AK Steel ASTM A 1011, Grade 55 Hot Rolled Carbon Steel, Structural Steel (SS)
Aluminum 6061-T6; 6061-T651

NZ97049 / 191448

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.