MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pyrotek TS-111 Thermoset Electrical Insulation Product (Nema Grade: G-11)
Categories: Polymer; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: Glass reinforcement, Epoxy Resin, Natural Color. Good electrical and mechanical properties.

Applications

  • Superstructure support pads
  • Bus bar insulators
  • Pot cradle insulators
  • Exhaust duct insulators
  • Machined parts
  • Wedges & shunts
  • Point feeder gaskets

Advantages

  • High insulation properties
  • High strength
  • Low moisture absorption
  • High temperature resistance

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.794 g/cc
Water Absorption 0.085 %
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 393 MPa
Compressive Strength 345 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+12 ohm-cm
Dielectric Strength 18.0 kV/mm
Arc Resistance 185 sec
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 160 °CContinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass
Owens Corning Glass Fiber Reinforced Polyester, Woven Roving (Lay-up), 50 wt.% glass
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 30 wt.% glass
Owens Corning Glass Fiber Reinforced Polyester (Spray-up/Lay-up), 30 wt.% glass
Budd BD-811, 40% Glass, High-Strength, Low-Shrink

PPYRO048 / 58381

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.