MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sawbones Solid Rigid Polyurethane Foam 50 pcf Density
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Solid Rigid Polyurethane Foam

Primary Use
Solid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mechanical properties of human bone, however, it does provide consistent and uniform material with properties in the range of human cancellous bone. Relevant mechanical properties for comparison to human cancellous bone may depend on the particular test method that is being developed.

The ASTM F-1839-08 "Standard Specification for Rigid Polyurethane Foam for Use as a Standard Material for Testing Orthopaedic Devices and Instruments" states that, "The uniformity and consistent properties of rigid polyurethane foam make it an ideal material for comparative testing of bones screws and other medical devices and instruments."

Description
Solid rigid polyurethane foam has a closed cell content ranging from 96.0 to 99.9%. Foam is available in a range of sizes and densities, from 0.08 to 0.80 grams per cubic centimeter (5 to 50 pounds per cubic foot).
.
Standard block size: 13cm X 18cm X 4cm
Standard sheet size: 13cm X 18cm X 3mm

Other Notes
Water absorption ranges from 0.301 to 0.0 kg/m2
Foam meets ASTM F-1839-08. Block dimensions are within ±2mm and sheet thickness is within ±0.3mm. Foam density may vary ±10%.
Properties parallel to direction of the rise of foam.

Information provided by Sawbones.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.800 g/cc0.0289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 27.0 MPa3920 psi
Tensile Modulus 1.469 GPa213.1 ksi
Compressive Yield Strength 48.0 MPa6960 psi
Compressive Modulus 1.15 GPa167 ksi
Poissons Ratio 0.300.30
Shear Modulus 0.178 GPa25.8 ksi
Shear Strength 16.0 MPa2320 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C
@Temperature -46.0 - 93.0 °C
35.0 µin/in-°F
@Temperature -50.8 - 199 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sawbones Solid Rigid Polyurethane Foam 40 pcf Density
Sawbones Second-Generation Simulated Cancellous Bone (Solid)
Mearthane Durethane™ M DM-630A Foam Polyurethane
Sawbones Solid Rigid Polyurethane Foam 30 pcf Density
Sawbones Cellular Rigid Polyurethane Foam 20 pcf Density

PSAWBO15 / 66546

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.