MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M 4412G Extreme Sealing Tape
Categories: Polymer; Tape

Material Notes: 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough yet flexible and abrasion resistant. The very soft and thick acrylic adhesive has excellent sealing properties and good outdoor durability. This single coated tape is designed to seal over an existing joint, seam, or penetration. The adhesive is designed to adhere well to the ionomer film so that overlapping tape joints can be made while maintaining a strong seal.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.820 g/cc
Thickness 2.00 milLiner
 4.00 milBacking
 76.0 milAdhesive
 80.0 milTotal
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 11.2 MPaD-412 dog bone die C; ASTM D3759
Elongation at Break 200 %D-412 dog bone die C; ASTM D3759
Peel Strength 16.0 pli
@Time 259000 sec
Adhesion to Glass; ASTM D3330
 17.0 pli
@Time 259000 sec
Adhesion to Truck Paint; ASTM D3330
 17.0 pli
@Time 259000 sec
Adhesion to Acrylic; ASTM D3330
 17.0 pli
@Time 259000 sec
Adhesion to PP; ASTM D3330
 18.0 pli
@Time 259000 sec
Adhesion to Stainless; ASTM D3330
 18.0 pli
@Time 259000 sec
Adhesion to Aluminum; ASTM D3330
 18.0 pli
@Time 259000 sec
Adhesion to PC; ASTM D3330
 18.0 pli
@Time 259000 sec
Adhesion to ABS; ASTM D3330
 18.0 pli
@Time 259000 sec
Adhesion to PVC; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.0 °CLong term
 149 °CShort term
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM34471 / 169218

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.