MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper Silicon Alloy, UNS C87850 , M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Sand Cast

Casting Characteristics: High – Fluidity; Medium – Casting Yield, Effect of Section Size, Shrinkage in Solidification; Low – Drossing, Gassing

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Hot Formed; Good Suitability – Oxyacetylene Welding, Spot Weld, Seam Weld, Butt Weld; Good Suitability – Capacity for Being Cold Worked

Typical uses: Valve Bodies for Water; Marine Products; Faucets; Plumbing Fittings; Water Meter Cases

Applicable Specifications: As Continuous Cast – ASTM B505/B505M; As Permanent Mold Cast – ASTM B806; As Sand Cast – ASTM B584; Ingot – ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.30 g/cc0.300 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 407 MPa>= 59000 psi
 434 MPa63000 psiTypical
Elongation at Break >= 16 %>= 16 %Typical
 25 %25 %
Tensile Modulus 105 GPa15200 ksi
Machinability 70 %70 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000220 ohm-cm0.0000220 ohm-cm8% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear  18.5 µm/m-°C
@Temperature 20.0 - 100 °C
10.3 µin/in-°F
@Temperature 68.0 - 212 °F
 18.5 µm/m-°C
@Temperature 20.0 - 200 °C
10.3 µin/in-°F
@Temperature 68.0 - 392 °F
 18.7 µm/m-°C
@Temperature 20.0 - 300 °C
10.4 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 3.14 W/m-K21.8 BTU-in/hr-ft²-°F
Melting Point 855.0 - 880.0 °C1571 - 1616 °F
Solidus 855.0 °C1571 °F
Liquidus 880.0 °C1616 °F
Annealing Point 500 - 600.0 °C932 - 1112 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Component Elements PropertiesMetricEnglishComments
Antimony, Sb <= 0.10 %<= 0.10 %
Copper, Cu 74 - 78 %74 - 78 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.090 %<= 0.090 %
Manganese, Mn <= 0.10 %<= 0.10 %
Nickel, Ni <= 0.20 %<= 0.20 %
Phosphorus, P 0.050 - 0.20 %0.050 - 0.20 %
Silicon, Si 2.7 - 3.4 %2.7 - 3.4 %
Tin, Sn <= 0.30 %<= 0.30 %
Zinc, Zn 17.6 - 23.3 %17.6 - 23.3 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC87850x3 / 292566

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.