MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos R08S-00 Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: This is a medium flow rate random copolymer designed for extrusion processing requiring slip properties and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

    Applications
  • Cast Film
  • Expanded PP Beads
  • Blow molding
  • Injection molding
  • Thermoforming

    Benefits
  • Superior slip properties
  • Consistent processing

Information provided by Ineos Olefins & Polymers USA

Key Words: Extrusion processing requiring slip properties
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.901 g/ccASTM D792
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 77Injection Molded; ASTM D785
Tensile Strength at Break 3600 psi2.0 in/min, Injection Molded; ASTM D638
Tensile Strength, Yield 3800 psi2.0 in/min, Injection Molded; ASTM D638
Elongation at Break >= 900 %2.0 in/min, Injection Molded; ASTM D638
Elongation at Yield 13 %2.0 in/min, Injection Molded; ASTM D638
Flexural Modulus, 1% Secant 123000 psiInjection Molded; ASTM D790A
Izod Impact, Notched 0.500 ft-lb/in
@Temperature 3.89 °C
Injection Molded; ASTM D256
 1.00 ft-lb/in
@Temperature 22.8 °C
Injection Molded; ASTM D256
Izod Impact, Notched (ISO) 1.33 ft-lb/in²
@Temperature 3.89 °C
Area, Injection Molded; ASTM D256
 2.52 ft-lb/in²
@Temperature 22.8 °C
Area, Injection Molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 174 °FUnannealed, Injection Molded; ASTM D648
Vicat Softening Point 269 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 60 %
@Thickness 1.27 mm
ASTM D1003
Gloss 92 %60°, Injection Molded; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ProcessExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Flint Hills P5M2Z-012 Polypropylene Random Copolymer
3M Dyneon™ FX 5929 Polymer Processing Additive
3M Dyneon™ Dynamar™ FX 5927 Polymer Processing Additive
Braskem RP 347 Injection Molding Polypropylene
Borealis RE420MO Polypropylene Random Copolymer, Transparent

PINEOS065 / 99386

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.