MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil Exxtral™ HMU 301 Performance Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Product Description: A specialty thermoplastic polyolefin resin designed for high heat and discoloration resistance, good surface finish, and detergent resistance for electrical appliances such as washing machines. Contains an anti-static additive.

Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America

Features:

  • Good Colorability
  • Good Dimensional Stability
  • Good Surface Finish
  • High Flow
  • Ultra High Stiffness
Uses:
  • Appliance Components
  • Appliances
  • Consume Applications
Processing Method: Injection Molding

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 230 °C
14 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 30.0 MPa4350 psiISO 527-2/50
Tensile Strength, Yield 33.4 MPa4840 psiISO 527-2/50
Elongation at Break 9.0 %9.0 %ISO 527-2/50
Elongation at Yield 3.0 %3.0 %ISO 527-2/50
Tensile Modulus 3.30 GPa479 ksiSecant; ISO 527-2
Flexural Modulus 3.30 GPa479 ksiISO 178
Charpy Impact, Notched 0.357 J/cm²
@Temperature 22.8 °C
1.70 ft-lb/in²
@Temperature 73.0 °F
Complete Break; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 63.9 °C147 °FISO 75-2/A

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Addiplast Addilene H 560 Polypropylene Homopolymer
ExxonMobil Exxtral™ HMU 216 Performance Polyolefin
Addiplast Addilene H 462 M20 Polypropylene Homopolymer
ExxonMobil Exxtral™ HMU 404 Performance Polyolefin
ExxonMobil Exxtral™ HMU 234 Performance Polyolefin

PEX99380 / 175616

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.