Description: SBR 1723 is an oil extended cold polymerization SBR with 37.5 parts of Low PCA (PolyCyclic Aromatic) oil and styrene-butadiene copolymer of 23.5% bound styrene. Raw materials for this product are carefully chosen for the best physical properties. The aromatic oil in SBR 1723 is an eco-friendly type (TDAE) which meets the European legislation on extender oil. Applications: SBR 1723 can be used in tire tread, camelback and other industrial products. CAS No: 9003-55-8 Information provided by LG Chemical |