MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arlon Electronic Materials 45NK Woven Kevlar® Reinforced Laminate and Prepreg
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: 45NK is a woven Kevlar® aramid fiber reinforced multifunctional epoxy laminate system engineered to provide in-plane CTE values as low as 6 ppm/°C for compatibility with leadless alumina ceramic chip carriers (LCCCs) and other low expansion SMT devices where control of laminate expansion is critical for solder joint reliability. 45NK exceeds the requirements of IPC-4101/50 (Type AFG).

  • High Tg (170°C) for improved reliability through process and in-use
  • Low Dielectric Constant 3.9
  • High modulus (19 Mpsi) p-aramid woven fiber reinforcement with CTE of -4 ppm/°C provides superior X-Y CTE of 5-7 ppm/°C
  • Process compatible with conventional high Tg multifunctional epoxy systems
  • 100% Organic resin/reinforcement system is suitable for laser drilling
  • RoHS/WEEE compliant

Typical Applications:

  • SMT Board Designs using LCCCs or other low expansion chip carriers
  • SMT Designs requiring both low in-plane CTE and laser drilling

    Information provided by ARLON Electronic Materials.

  • Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

    Click here to view all available suppliers for this material.

    Please click here if you are a supplier and would like information on how to add your listing to this material.

     
    Physical PropertiesOriginal ValueComments
    Density 1.50 g/ccASTM D792 Method A
    Water Absorption 0.80 %IPC TM-650 2.6.2.1
     
    Mechanical PropertiesOriginal ValueComments
    Modulus of Elasticity 4000 ksiIPC TM-650 2.4.18.3
    Poissons Ratio 0.20ASTM D3039
    Peel Strength 6.00 pliTo Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8
     6.00 pliTo Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8
     6.00 pliTo Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity 1.30e+13 ohm-cmC96/35/90; IPC TM-650 2.5.17.1
    Surface Resistance 3.20e+13 ohmC96/35/90; IPC TM-650 2.5.17.1
    Dielectric Constant 3.9
    @Frequency 1e+6 Hz
    may vary with resin %; IPC TM-650 2.5.5.3
    Dielectric Strength >= 750 V/milIPC TM-650 2.5.6.2
    Dissipation Factor 0.016
    @Frequency 1e+6 Hz
    IPC TM-650 2.5.5.3
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 5.00 - 7.00 µm/m-°CIPC TM-650 2.4.41
    CTE, linear, Transverse to Flow 75.0 µm/m-°Cz, below Tg; IPC TM-650 2.4.24
     225 µm/m-°Cz, above Tg; IPC TM-650 2.4.24
    Thermal Conductivity 0.220 W/m-KASTM E1461
    Glass Transition Temp, Tg 170 °CDSC; IPC TM-650 2.4.25
    Flammability, UL94 V-0
     
    Descriptive Properties
    Z-Axis Expansion (%)2.8IPC TM-650 2.4.24 (50-260°C)

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Solvay CYCOM® 5250-4 BMI Prepreg System with IM7-6K-5HS Woven Carbon Fiber
    Overview of materials for Epoxy/Carbon Fiber Composite
    G-10 Fiberglass Epoxy Laminate Sheet
    Solvay CYCOM® 950-1 Epoxy Prepreg with 52% 285 Kevlar Fabric
    DuPont™ Nomex® Type 994, 125 mil Nominal Thickness Rigid Aromatic Nylon Board

    PARLM9881 / 149034

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.