Hostacom DRC725D BLK high melt flow, 1,300 MPa flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of properties and processability. It is typically used for painted applications that require a good balance of rigidity and low temperature impact performance. Applications: Automotive Parts, Exterior Automotive Applications.Information provided by LyondellBasell. |