MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC SABIC® PP 519A PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PP 519A is a polypropylene homopolymer resin specifically designed to enable optimised production speed of very fine filament titre resulting in an excellent balance of mechanical properties and softness. The rheological performance of SABIC® PP519A is providing the potential to optimise production efficiency especially for fibre production characterised by consistent high speed and low non wovens weights at reduced temperatures. SABIC® PP 519A has a very narrow molecular weight distribution. SABIC® PP 519A is compatible with all existing spun bond machine technologies producing different non woven compositions. SABIC® PP 519A has a special developed anti gas fading formulation to minimise discolouration of the fibers.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 30.0 MPaISO 527-2 1A
Elongation at Yield 10 %Speed of testing: 50 mm/min; ISO 527-2 1A
Tensile Modulus 1500 MPaSpeed of testing: 1 mm/min; ISO 527-2 1A
 
Descriptive Properties
Gas fading stabilizedTrueSABIC method
IsotacticityMedium
Molecular Weight DistributionNarrow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11188 / 244655

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.