MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® 940G Nylon 66, Extrusion Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Extruded; Nylon 66, Film

Material Notes: 940G is a PA66-based terpolymer that features high melt strength/shear thinning behavior ideal for multilayer film, high strength, ductility, and slow crystallinity that matches crystallization temperatures very close to that of ethylenes. The slow crystallization behavior coupled with the melting point ~ 215-220°C and great mechanical properties makes this material extremely useful for outside layers or internal layers of the multilayer film. This material further exhibits a very high elongation to break (> 600%) allowing for high draw ratios for thermoforming or when orienting the film. The high elongation and high clarity/gloss is further useful for monofilament applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.674 g/ccASTM D1895
Density 1.14 g/ccISO 1183
Moisture Absorption 0.100 %ASTM D6869
Viscosity Measurement 3.8 - 4.1Relative Viscosity - Sulfuric Acid; ISO 307
 115 - 145Relative Viscosity - Formic Acid; ASTM D789
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD >= 600 %
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D882
Film Elongation at Break, TD >= 600 %
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D882
Elmendorf Tear Strength MD 100 g
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D1922
Elmendorf Tear Strength TD 140 g
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D1922
Dart Drop Test >= 2000 g
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D1709A
Film Tensile Strength at Break, MD 97.0 MPa
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D882
Film Tensile Strength at Break, TD 97.0 MPa
@Thickness 0.0380 mm
Cast Film, Conditioned; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 216 °CISO 11357-3
Crystallization Temperature 130 °CISO 11357-3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 40.0 °CBlow Film Air Temperature
 245 - 265 °CCylinder - Extrusion
Die Temperature 250 - 275 °CExtrusion
 70.0 - 80.0 °C
@Time 0.000 - 14400 sec
Extrusion
Melt Temperature 216 °CExtrusion
Moisture Content 0.030 - 0.080 %Extrusion
 
Compliance PropertiesOriginal ValueComments
European Food 1935/2004 Yes
 
Descriptive Properties
Agency RatingsEU 10/2011
 EU 2023/2006
FeaturesGood Chemical Resistance
 Heat Stabilized
 High Melt Stability
 High Melt Strength
 High Strength
 High toughness
 Puncture Resistance
Melt Pressure MPa3-17
Screw DesignGP or Barrier
UsesIndustrial Applications
 Monofilaments
 Multilayer Film
 Profiles
 Rods
 Sheet
 Tubing
 Vacuum Bagging Film

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon 25188T010 Silicone Rubber/Laminated ETFE Film

PZASCE9776 / 220879

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.