MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Visit Zeus Inc. for Fluoropolymer Tubing

(Viewing data as-entered. Click here to return)
Zeus Absorv® Polydioxanone (PDO) Bioabsorbable Polymer
Categories: Polymer

Material Notes: Absorv® Bioabsorbable products are particularly suitable for medical applications seeking to provide an alternative to metal stents or other components. A key advantage of bioabsorbable polymers over other materials is their innate ability to be absorbed naturally by the body, eliminating the need for permanent device implantation or for surgical removal at a later date.

Zeus can select, blend, and process various bioabsorbable polymers to produce high precision tubular geometries, monofilaments, special profiles, ribbons, and microporous non-woven fabrics for use in a number of clinical applications across multiple disciplines including coronary and peripheral vascular intervention, structural heart intervention, drug delivery, brachytherapy, gastroenterology, and otolaryngology (ENT).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 65.0 MPa
Modulus of Elasticity 0.400 - 1.00 GPa
 
Thermal PropertiesOriginal ValueComments
Melting Point 100 - 110 °C
Glass Transition Temp, Tg -10.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Total Mass Lost5-9 MonthsApproximate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZEUS971m / 323356

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.