MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company Permaprene™ 2800 B-85A Thermoplastic Polyolefin Elastomer (TEO)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccASTM D 792
Linear Mold Shrinkage 0.013 - 0.019 cm/cm
@Thickness 3.20 mm
0.013 - 0.019 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 858510 s delay; ASTM D 2240
Tensile Strength at Break 10.3 MPa1500 psiDie C, 0.125 in (3.2mm); 20 in/min (500 mm/min); ASTM D 412
Tensile Strength, Yield 6.07 MPa880 psiDie C 0.125 in (3.2 mm); 20 in/min (500 mm/min); 100%; ASTM D 412
Elongation at Break 750 %750 %Die C, 0.125 in (3.2mm); 20 in/min (500 mm/min); ASTM D 412
Tear Strength 49.1 kN/m280 pliDie C; ASTM D 624
Compression Set  35 %
@Temperature 23.0 °C,
Time 79200 sec
35 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 56 %
@Temperature 70.0 °C,
Time 79200 sec
56 %
@Temperature 158 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 227 °C380 - 440 °F
Mold Temperature 21.1 - 79.4 °C70.0 - 175 °F
Drying Temperature 79.4 °C
@Time 7200 - 10800 sec
175 °F
@Time 2.00 - 3.00 hour
Moisture Content <= 0.050 %<= 0.050 %
Dew Point -17.8 °C0.000 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer
RTP Company Permaprene™ 2800 B-65A Thermoplastic Polyolefin Elastomer (TEO)
Multibase Multi-Flex® D 5308 HF Black TPO Thermoplastic Polyolefin Elastomer
Multibase Multi-Flex® D 5308 848 Black TPO Thermoplastic Polyolefin Elastomer
Multibase Multi-Flex® D 5304 Black TPO Thermoplastic Polyolefin Elastomer

PQZRA37089 / 206143

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.