MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beijing Evergrow Resources Glass Filled Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes:

Information provided by Beijing Evergrow Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccGB1033
Water Absorption 3.5 - 4.1 %
Moisture Absorption 1.65 - 1.83 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85 - 90GB3398
Ball Indentation Hardness 175 MPaGB3398
Tensile Strength at Break 130 - 150 MPaGB/T 1040
Elongation at Yield <= 20 %GB/T 1040
Modulus of Elasticity 6.90 GPaGB/T 1040
Flexural Strength 150 MPaGB9341
Compressive Strength 110 - 130 MPaGB/T 1040
Izod Impact, Notched (ISO) 5.50 kJ/m²GBT1043
Coefficient of Friction 0.45GB3360
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 ohm-cmVolume; GB1410
Arc Resistance 475 secASTM D112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µm/m-°CGB1036
Melting Point 260 °CHG/T2235
Heat Distortion Temperature 150 °CGB1634

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK)
Overview of materials for Polycarbonate, 20% Glass Filled
Beijing Evergrow Resources MC Nylon
Eurotec® Tecomid® NAX0 GR70 NL HS PA6.6, 70% glass fiber reinforced, heat stabilized, natural
Ensinger Tecapeek® XP-96 Compression Molded PEEK

PBEIJ110 / 90179

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.