MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
The Chemical Company Methanol
Categories: Fluid; Solvent

Material Notes: Methanol is a liquid chemical with the formula CH3OH (often abbreviated MeOH). It is colorless, volatile, flammable, and poisonous. Methonal is made from the destructive distillation of wood and is chiefly synthesized from carbon monoxide and hydrogen. Its principal uses are in organic synthesis, as a fuel, solvent, and antifreeze. Methanol is toxic. Drinking 10 ml of the substance will cause blindness; consuming as little as 100 ml will result in death. It is the simplest form of alcohol and has a distinctive odor that is similar to ethanol (drinking alcohol), but slightly sweeter. Methanol is a polar liquid at room temperature. It is used as antifreeze, solvent, fuel, and as a denaturant for ethanol. The chemical is also used to produce biodiesel via transesterification reaction. Because Methanol has toxic properties, it is frequently used as a denaturant additive for ethanol manufactured for industrial purposes. Methanol is frequently called wood alcohol because it was once produced primarily as a byproduct of the destructive distillation of wood. Today, three methods are commonly used to produce synthesis gas from the methane component in natural gas. The methods are steam-methane or SMR, which is endothermic, partial oxidation with molecular oxygen, which is exothermic, and the combination of the two, which is referred to as autothermal reforming.

Information provided by The Chemical Company

Key Words: hydroxymethane; methyl alcohol; methyl hydrate; wood alcohol; carbinol; CAS Number 67-56-1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.791 - 0.793 g/cc
@Temperature 20.0 °C
Brookfield Viscosity 0.59 cP
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 3.0wt% acetic acid
 
Thermal PropertiesOriginal ValueComments
Melting Point -97.0 °C
Boiling Point 64.7 °C
Distillation Temperature <= 1.00 °C
@Pressure 0.101 MPa
including 64.6 ± 0.1
Flash Point 12.0 °Cclosed cup
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl <= 0.050 %
Iron, Fe <= 0.010 %
Sulfur, S <= 0.050 %
 
Descriptive Properties
Acetone (mg/kg)< 30
Alcohol Content50mg/kgEthanol
AppearanceClear liquid, free of suspended matter
Assay= 99.85%
Carbonizable Substances [Pt-Co Scale]< 30
Hazen Color Value (pt-co)< 5
HydrocarbonsPass
Permanganate Time (min)< 815°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1016 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
Teknor Apex Sinvicomp SSG 5003 Polyvinyl Chloride, Flexible
CoreLite BALSASUD® Core UL Ultra Lite Balsa Core Material
Carbon-Core Carbon Balsa Wood
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2

PTCC010 / 106999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.