MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SCIGRIP SG305 A Methacrylate Adhesive + SG605 B Activator
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: SCIGRIP® SG300 Series Methacrylate Adhesives are two-component, 10:1 mix ratio products for bonding metals, composites and other plastic parts. Most metals can be bonded without primer. These advanced products are designed to meet specific requirements of the transportation industry, including reduced read through on show surfaces. The combination of minimum surface preparation, primerless metal bonding and low read through makes the SG300 series products ideal for a variety of assembly operations.

Features: Reduced bond line read through; Minimal surface preparation; Non-sag application; Excellent environmental resistance; Excellent fatigue, impact and shock load resistance.

Information provided by SCIGRIP Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccAdhesive
 1.02 g/ccMix
 1.12 g/ccActivator
Viscosity 120000 - 180000 cPActivator
 175000 - 275000 cPAdhesive
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1.70 - 2.20 ksi
Elongation at Break 40 - 60 %
Tensile Modulus 30.0 - 40.0 ksi
Adhesive Bond Strength 2300 - 2800 psiLap Shear
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 - 20.0 min
@Temperature 23.9 °C
Fixture Time
Working Life 4.00 - 6.00 min
@Temperature 23.9 °C
 
Descriptive Properties
ColorBlack or Off WhiteActivator
 Black or Off WhiteMix
 Off WhiteAdhesive
Mix Ratio10:1 A:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCIGR961 / 243185

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.