DURAFILL MXF121 is an amorphous, opaque Copolyester with mold release. It offers toughness, hydrolytic stability, heat resistance, chemical resistance, and melt flowability. This product is designed for medical device applications. It is ISO10993 compatible for cytotoxicology, skin sensitization, and intracutaneous reactivity. It is available in colors. It is available in AMR, EUR, and PAC.Information provided by Conventus Polymers LLC |