MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Washington Penn Polypropylene Copolymer 20% Glass Reinforced, 11 MFI
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. The glass-reinforcement provides a better strength and modulus than any of the particulate mineral fillers.

Information provided by Washington Penn Plastic Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccASTM D792
Filler Content 20 %
Melt Flow 11 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 6800 psiASTM D638
Elongation at Break 14 %ASTM D638
Elongation at Yield 11 %ASTM D638
Flexural Modulus 350 ksiTangent; ASTM D790
Flexural Modulus, 1% Secant 330 ksiASTM D790
Izod Impact, Notched 4.00 ft-lb/inASTM D256
Gardner Impact 16.0 in-lb
@Temperature 23.0 °C
ASTM D5420
Impact 3.8Dynatup Impact, in/in; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 300 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 240 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Washington Penn Homopolymer Polypropylene 20% Glass Reinforced
Washington Penn Polypropylene Copolymer 20% Glass Reinforced, 15 MFI
Washington Penn Homopolymer Polypropylene 27% Glass Reinforced
Washington Penn Homopolymer Polypropylene 40% Glass Reinforced
Washington Penn Polypropylene Copolymer 30% Glass Reinforced

PWPP27 / 72810

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.