MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kraton® D0243 E (SBS) Diblock Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D0243 E polymer is a clear, diblock copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical form identified:
Kraton D0243 ET - supplied as a porous pellet dusted with talc

Region: Asia Pacific, Europe, Japan, North America and South America

Uses: Kraton D0243 E is used as a modifier of bitumen or thermoplastics and in compound formulations. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants and coatings

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing.

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccISO 2781
Volatiles <= 0.30 %KM 04
Ash 0.20 - 0.50 %ET; ISO 247
 
Chemical PropertiesOriginal ValueComments
Diblock Content 75 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70
@Time 10.0 sec
Estimated value; ISO 868
Tensile Strength 2.00 MPaEstimated value; ISO 37
300% Modulus 0.00100 GPa
@Strain 300 %
Estimated value; ISO 37
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.35-0.48%, KM 08
 Polystyrene30-34%, KM 03
 Total Extractables<1.0%, KM 05
 Vinyl35%, KM03

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D1118 K (SBS) Diblock Copolymer
Kraton® FG1901 + PA-6 blend (20/80)
Kraton® FG1901 + PBT blend (30/70)
Kraton® G1702 + PPE blend (20/80)
Kraton® D1184 A (SBS) Branched Block Copolymer

PKRA9801 / 132700

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.