Product Description: Key Features- 35-mesh powder
- Good moldability
- Excellent long term outdoor weatherability (UV8)
- Balance of toughness and rigidity
- Excellent low temperature impact
- Excellent environmental stress crack resistance, ESCR
- Compounded for uniform additive dispersion
- Natural as well as standard, custom or special effect colors available
- Stock colors may be available. See Stock color bulletin
- UL component recognition listing (E141240)
- Also available in powder form as HMP-305
Availability: North America Features: Good Moldability; Good Stiffness; Good Toughness; Good Weather Resistance; High ESCR (Stress Crack Resist.); High Rigidity; Low Temperature Impact Resistance UL File Number: E141240 Appearance: Colors Available; Natural Color; Opaque Form: Powder Processing Method: Rotational Molding Information provided by Ravago Manufacturing Americas |