MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ STAT-KON™ Compound DX05301C Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DX05301C compound is based on Polycarbonate (PC) resin containing conductive carbon powder. Added features of this grade include: LNP Clean Compounding Technology, Low Ionic, Low Outgassing, Low LPC and Electrically Conductive.

Features: LNP Clean Compound Technology,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
Density 1.22 g/cc0.0441 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity 22 cP
@Load 5.00 kg,
Temperature 300 °C
22 cP
@Load 11.0 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inSABIC method
Melt Flow 22.6 g/10 min
@Load 5.00 kg,
Temperature 300 °C
22.6 g/10 min
@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 56.0 MPa8120 psi5 mm/min; ISO 527
 60.0 MPa8700 psi5 mm/min; ASTM D638
Tensile Strength, Yield 48.0 MPa6960 psi5 mm/min; ASTM D638
 56.0 MPa8120 psi5 mm/min; ISO 527
Elongation at Break 1.5 %1.5 %5 mm/min; ISO 527
 9.9 %9.9 %5 mm/min; ASTM D638
Elongation at Yield 1.5 %1.5 %5 mm/min; ISO 527
 5.3 %5.3 %5 mm/min; ASTM D638
Tensile Modulus 2.49 GPa361 ksi1 mm/min; ISO 527
 2.59 GPa376 ksi5 mm/min; ASTM D638
Flexural Strength 77.0 MPa11200 psiyield, 2 mm/min; ISO 178
 95.0 MPa13800 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.28 GPa331 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.48 GPa360 ksi2 mm/min; ISO 178
Izod Impact Notched 54.0 J39.8 ft-lbASTM D256
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1e+05 - 4.50e+8 ohm-cm1e+05 - 4.50e+8 ohm-cmASTM D257
Surface Resistance 1e+05 - 4.50e+8 ohm1e+05 - 4.50e+8 ohmASTM D257
Static Decay <= 0.10 sec<= 0.10 sec5000V to <50V; FTMS101B
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 131 °C268 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 132 °C
@Thickness 3.20 mm
270 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 146 °C295 °FRate B/120; ISO 306
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.00 mm
HB
@Thickness >=0.0394 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81254 / 289201

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.