Availability: Asia Pacific; Europe; North America Fillers/Reinforcement: Glass Fiber, 30% Filler by Weight Features: Good Dimensional Stability; Pleasing Surface Appearance Form: Pellets Processing Method: Injection Molding Information provided by Teknor Apex |